Koz Ross on Nostr: nprofile1q…726sn Just finished and measured the 280C run. The matte zone transition ...
nprofile1qy2hwumn8ghj7un9d3shjtnddaehgu3wwp6kyqpq2atwfrq4rfv7fqara6gzsgrgj7k8ngewzl5nzs46agwyxzh0e25q6726sn (nprofile…26sn) Just finished and measured the 280C run. The matte zone transition was essentially in the same place (_maybe_ a tenth of a mm difference?), while the maximum went from 30ish VF to 32is VF. In reality, I'd say that the difference is essentially non-existent: both of those could be measuring errors for all I know.
I'll likely stick with 280C, and cap at 15VF to stay in the gloss zone for maximum layer adhesion. Next, PA and EM. (8/?)